The same properties of rubber but lighter.
Unmatched advantages
- The same feel as rubber.
- Excellent abrasion resistance, similar to vulcanized rubber.
- Easier and faster production than vulcanized and synthetic rubber.
- 40% lighter than typical rubber.
- Product rated as anti-slip.
- Does not require investment in production and equipment for producers of polyurethane shoe soles.
| Properties | PUcaucho® | Vulcanized Rubber | Thermoplastic Rubber |
|---|---|---|---|
| Density (g/cm3) | 0,70 - 1,10 | 1,10 - 1,30 | 0,95 - 1,00 |
| Hardness (Shore A) | 48 - 70 | 65 - 70 | 60 - 65 |
| Tensile strength (N/mm2) | 5 - 11 | 10 - 12 | 5 - 7 |
| Tear resistance (N/mm2) | 5 - 12 | 10 - 13 | 8 - 10 |
| Abrasion (mg) | 30 - 200 | 150 - 200 | 200 - 250 |
| Demoulding time (seg) | 30 - 240 | 480 - 600 | 240 - 400 |
| Resistencia a la flexión (Kciclos) | > 30 | > 30 | > 30 |
| PUcaucho® | |
|---|---|
| Density (g/cm3) | 0,70 - 1,10 |
| Hardness (Shore A) | 48 - 70 |
| Tensile strength (N/mm2) | 5 - 11 |
| Tear resistance (N/mm2) | 5 - 12 |
| Abrasion (mg) | 30 - 200 |
| Demoulding time (seg) | 30 - 240 |
| Resistencia a la flexión (Kciclos) | > 30 |
| Vulcanized Rubber | |
| Density (g/cm3) | 1,10 - 1,30 |
| Hardness (Shore A) | 65 - 70 |
| Tensile strength (N/mm2) | 10 - 12 |
| Tear resistance (N/mm2) | 10 - 13 |
| Abrasion (mg) | 150 - 200 |
| Demoulding time (seg) | 480 - 600 |
| Resistencia a la flexión (Kciclos) | > 30 |
| Thermoplastic Rubber | |
| Density (g/cm3) | 0,95 - 1,00 |
| Hardness (Shore A) | 60 - 65 |
| Tensile strength (N/mm2) | 5 - 7 |
| Tear resistance (N/mm2) | 8 - 10 |
| Abrasion (mg) | 200 - 250 |
| Demoulding time (seg) | 240 - 400 |
| Flexion resistance (Kciclos) | > 30 |